CHEMUNI联合化学Polycarboxylate ethers

Product range

Six grades, one molecular logic.

From the water-reducing grade to the shrinkage-reducing one, the difference is not a ranking — it is which anchor group and side-chain length fits your materials. Selection first, data sheets after.

Choose by problem, not by SKU

Your constraint Grade Why
Highest water reduction, short haulCU-100highest grafting density; best cost per unit of water reduced
Retention beyond two hours, or hot weatherCU-200slow-release anchoring, progressive adsorption
Cold weather, fast demouldingCU-300early strength without chloride
Clay-bearing sand, high methylene blue valueCU-400sacrificial anchor protects the dispersing polymer
High-strength, SCC, high pump pressureCU-500lower plastic viscosity, shorter T500
Floors, decks, linings — cracking is the riskCU-600lowers 90-day drying shrinkage

When two constraints apply at once, blend rather than pick: CU-100 with CU-200 from 30:70 to 50:50 covers water reduction and retention together.

Data by grade

Typical values, measured at 25 °C

CU-100

Water-reducing

High water reduction, balanced set.

The workhorse grade. A high grafting-density polycarboxylate for ready-mixed concrete where the priority is water reduction and strength, and haul times are short. At equal slump the mix water can usually be cut by 30–40 %, which is where the cement saving and the strength gain both come from.

  • Water reduction of 30–40 % at equal slump, at 0.15–0.45 % of binder
  • Minimal effect on setting time at recommended dosage
  • Blends with retarders and air-entraining agents; compatibility confirmed by trial
  • Supplied at 50 % solids, with 40 % and 60 % on request

Typical use · Ready-mixed concrete, general structural work, pumped concrete.

CU-200

Retain

Slump retention over long hauls and hot weather.

Built on a slower-hydrolysing anchor. The polymer reaches the particle surface progressively over the first two hours instead of all at once, so a mix that sits in traffic or waits at the pump still flows when it arrives. Intended for 2–3 h retention; setting time is retarded by roughly 30–90 min at typical dosage and should be checked against the stripping and finishing schedule.

  • Slump retention to 2–3 h at 25–35 °C ambient
  • Progressive adsorption keeps initial bleeding risk low
  • Blend with CU-100 from 30:70 to 50:50 to tune retention to the haul
  • Slight retardation — verify against formwork stripping and finishing windows

Typical use · Long-haul ready-mix, hot-weather casting, staged pours, pumped high-rise.

CU-300

Early

Earlier strength, no chloride.

For precast demoulding, cold-weather casting and fast-track repair. Some water reduction is traded for a denser early hydration response, so 12–24 h strength comes up at equal cement content. Chloride content stays below 0.05 %, which keeps the mix inside the reinforcement limits of GB 8076 without an extra corrosion argument.

  • Raises 12–24 h strength at equal cement content
  • Chloride-free; no corrosion risk added to the reinforcement
  • Stable under 5–15 °C placing conditions
  • Works with CU-200 when both early strength and retention are needed

Typical use · Precast demoulding, winter concreting, repair mortars, fast-track pavement.

CU-400

Clay-tolerant

Tolerance to clay-bearing sand and aggregate.

Sand carrying montmorillonite or illite adsorbs polyethylene oxide side chains and removes the polymer from the pore solution before it ever reaches the cement. CU-400 carries a sacrificial adsorption block: clay consumes that first and the dispersion work continues. For aggregate with a methylene blue value above 1.4 g/kg, most of the lost slump can usually be recovered — measured in a trial, not assumed.

  • Sacrificial anchor protects the dispersing polymer from clay uptake
  • Recovers workability with high-MB manufactured sand
  • Reduces the dosage penalty of dirty aggregate
  • Same handling and storage as the standard grades

Typical use · Manufactured sand, recycled aggregate, quarries with variable clay content.

CU-500

Viscosity-reducing

Lower plastic viscosity in low w/b and self-compacting mixes.

High-strength mixes, SCC and long-boom placements running at a low water/binder ratio are not short of flow — they are short of flow rate. CU-500 acts on the rheology rather than on yield stress alone: at the same slump flow the mix spreads further, T500 comes down and the pump pressure with it. It is the grade to reach for when the paste is too stiff for the aggregate grading in hand.

  • Lowers plastic viscosity at equal slump flow — T500 comes down
  • Cuts pump pressure on long booms and high-rise placements
  • Holds segregation resistance when used alongside a VMA
  • Supplied as finished admixture; mother liquor available for blenders

Typical use · High-strength concrete, SCC, mass pours, long-distance pumping, low w/b precast.

CU-600

Shrinkage-reducing

Lower drying shrinkage, fewer restraint cracks.

For slabs, floors, bridge decks and tunnel linings, where the crack that matters is the one that opens months after casting. The polymer lowers the surface tension of the pore solution and slows water loss from the capillary network, so 90-day drying shrinkage comes down against the same mix without it. Water reduction is kept moderate on purpose: an over-plasticised mix bleeds less, shrinks more, and defeats the point.

  • Lower 90-day drying shrinkage against the same mix without it
  • Moderate water reduction — far less than CU-100 by design
  • Chloride-free, no added sulfate; safe in reinforced concrete
  • Blends with CU-200 where retention is also short

Typical use · Ground slabs, industrial floors, bridge decks, tunnel linings, liquid-retaining structures.

About these numbers

The ranges above are typical values for the grade under standard conditions. They exist for comparison during selection, not as a specification. The contractual specification is the TDS agreed between us; delivery is governed by the COA of the batch. Where the two differ, the COA governs, handled under the contract terms.

Dosages are percentages by mass of binder. The working dosage has to come from a trial: C₃A and alkali content of the cement, the SCM ratio, and the clay content and grading of the sand will make the same grade behave differently at two plants.

Packing and delivery

Standard packing is a 1,000 L IBC, a 200 L drum, or a flexitank in a 20′ container; mother liquor can go bulk. A 20′ container typically takes 18–20 IBCs or 80 drums, confirmed against destination weight limits and carrier rules.

Packaging and loading plans →

Not sure which grade?

Send the cement report and the mix design. One trial usually narrows it to two grades, with a blend ratio.