Technology

Dispersion is not a thinner you pour in. It is interfacial chemistry you design.

Three things decide how your concrete behaves at the pump: how the molecule adsorbs, how the side chains hold particles apart, and what you change when the materials change.

01 · Mechanism

Two mechanisms in one molecule

Cement particles flocculate in water under surface charge and van der Waals attraction, locking free water inside the flocs. A water reducer releases that water — not by adding water, but by keeping the particles apart.

Anionic plasticisers — lignosulfonate, naphthalene — rely on electrostatic repulsion: after adsorption the particles carry the same charge and push apart. The charge is screened by ions in the pore solution and decays with time, and once the adsorption sites are filled, more admixture adds nothing.

A polycarboxylate adds steric hindrance on top of that. Carboxylates anchor to the surface; PEO side chains stay hydrated and reach into the liquid. When particles come close enough for the chains to overlap, water is expelled from between them and the resulting osmotic and elastic penalty pushes the particles back. That force is not screened by ionic strength, so it works at low dosage, and how long it lasts is set by side-chain structure and hydrolysis rate.

BACKBONE PEO SIDE CHAINS –COO⁻ anchor CEMENT PARTICLE SURFACE
Backbone anchored, side chains extended. Adsorbed amount and barrier thickness are independently adjustable — the design space that earlier generations did not have.

A constraint that gets overlooked

Water reduction and retention compete for the same adsorbed amount. The harder the initial dispersion, the less polymer is left for later. "High reduction and long retention" comes from blending and slow-release design, not from one molecule doing both at its limit.

02 · Molecular design

Five levers, each with a price

Lever What it changes What it costs
Side-chain length (EO units)Thickness of the steric barrier. Longer chains hold particles further apart and retain slump better, at higher paste viscosity.Slower adsorption; past a point, water reduction falls.
Acid-to-ether ratio (anchor density)Carboxylate density sets how fast and how firmly the polymer adsorbs. A high ratio gives strong initial dispersion.Adsorbing too fast spends the retention budget and increases sulfate sensitivity.
Molecular weight and distributionSet by initiator and chain-transfer agent dose. Mid-range molecular weight disperses most efficiently.Too high bridges particles and bleeds; too low does not anchor.
Functional monomersHydrolysable esters give slow-release retention; amides and silanes improve clay tolerance and bleeding control.Hydrolysis depends on temperature and alkalinity; the formulation must be calibrated for the climate.
Neutralisation and solidsSets pH, storage stability, and compatibility with blend partners.Low pH attacks packaging; high pH is incompatible with some retarders.

This table is the language we use with customers. When someone says the mix is not flowing, the useful question is which part is not flowing — at discharge, at one hour, or at two. Different answers move different levers.

03 · Synthesis

Aqueous free-radical copolymerisation, a handful of control points

MonomersAPEG · TPEG · HPEGCopolymeriseredox · 55–65 °CNeutraliseNaOH → pH 6–8ReleaseCOA per batch
The standard route. The difference is in the control: feed rate sets the molecular weight distribution, chain-transfer agent sets the molecular weight, and the end point sets residual monomer.

Molecular weight

Set by the ratio of initiator to chain-transfer agent (thioglycolic or 3-mercaptopropionic acid). Too high bridges particles and bleeds; too low fails to anchor. The tighter the batch-to-batch band, the less a blender has to re-tune.

Residual monomer

Unreacted monomer is both lost performance and an odour and compliance issue. Held below 0.1 % at release through hold time and post-initiation, and measured on every batch.

Neutralisation and solids

Neutralised to pH 6–8 with NaOH or KOH for storage stability and blend compatibility. High-solids liquor (60 %) thickens noticeably in the cold — winter shipments are assessed route by route.

04 · Compatibility and troubleshooting

The seven situations that come up most

Symptom Likely cause Action
Slump loss over 60 mm in one hourHigh C₃A or alkali in the cement, or a sulfate shortage that consumes the polymer early.Move to CU-200 or blend with CU-100; check the sulfate carrier and make up the sulfate balance.
Bleeding, segregation, sticky mixOverdosing, a shortage of fines, or too high a water/binder ratio.Reduce the dose; raise the sand ratio or SCM content; add a VMA where needed rather than more admixture.
Retarded setExcess retarder, or cold placing conditions.Cut the retarder dose; substitute CU-300 for part of the retaining grade; work from measured set times.
High air content, large surface bubblesShear-entrained air that is not released, or stacking with an air-entraining agent.Add a defoamer; re-check the air-entraining dose; inspect the pump line for air ingress.
Works with one sand, fails with the nextMontmorillonite in the sand adsorbs the PEO side chains before the polymer reaches the cement.Switch to CU-400; grade incoming sand by methylene blue value; add a clay inhibitor where needed.
Incompatible with naphthalene or sulfamate admixturesTwo anionic polymers compete for adsorption, and residue in shared tanks destabilises the blend.Separate tanks and lines; flush before switching; run a compatibility test before any shared storage.
Diluted product precipitates or goes offDilution with hard water, or microbial growth.Dilute with deionised or softened water; mix to use; add biocide and store out of sunlight.

Rule out everything that is not the admixture

Dosing pump error, residue in the line, cement temperature, uncorrected sand moisture — these four account for more "admixture problems" than formulation does. Our on-site sequence is dosing and aggregate first, cement and SCMs second, formulation last.

A specific compatibility problem?

Send the cement analysis, the methylene blue value of the sand, your current dose, and the slump at discharge and on arrival. Most cases do not need a different product — only a different blend ratio.